No.145-A/No.145-B Specification
| Model | No.145-A CREEP TESTER (PULLEY TYPE) |
No.145-B CREEP TESTER (BALANCE TYPE) |
|---|---|---|
| Hangings | 3, 6, or 10 Hangings (3 kinds) | 3, 6, or 10 Hangings (3 kinds) |
| Specimen | See JIS-K7162 for reference JIS-K7162 | See JIS-K7162 for reference JIS-K7162 |
| Load Method | Pulley Wheel Type | Balance Scale Type |
| Weight Load | Max. 500 N (50 kgf) | Max. 5 kN (500 kgf) |
| Displacement Measurement | Magnetic Linear Scale 1/100 mm,Stroke 0 to Max. ± 150 mm | Magnetic Linear Scale 1/100 mm,Stroke 0 to Max. ± 40 mm |
| Temperature Range | Max. 200 °C | Max. 200 °C |
| Software | Windows Compatible | Windows Compatible |
| Option | Compression Jig, Bending Jig, Low Temperature Oven, Constant Temperature & Humidity Oven, Divided Oven, Liquid Immersion Bath, Gauge Length Measuring Spec, Weight Traveling System (WTS) |
Compression Jig, Bending Jig, Low Temperature Oven, Constant Temperature & Humidity Oven, Divided Oven, Liquid Immersion Bath, Gauge Length Measuring Spec, Weight Traveling System (WTS) |
| Power Source | Differ by Specifications. | Differ by Specifications. |
| Dimensions/ Weight (Approx.) | Differ by Specifications. | Differ by Specifications. |